Place of Origin: | Shandong |
Brand Name: | Hanwu |
Certification: | ISO ,BV ,SGS, CE |
Minimum Order Quantity: | 1 tons |
Packaging Details: | water proof paper is inner packing, galvanized steel or coated steel sheet is outer packing , side guard plate , then wrapped by seven steel belt. |
Delivery Time: | 15-20 days or subject to the clients' requirement and quantity |
Payment Terms: | 30%TT for deposit, 70% balance before shipment or LC at sight |
Supply Ability: | 20000 tons per month |
201 stainless steel is composed primarily of iron with between 16 and 18% chromium and up to 0.15% carbon. It also contains small amounts of manganese, nickel, silicon, nitrogen, and copper. It has higher formability than the 300 series grades. In addition, it can be hardened by cold working processes but not heat-treated like 304 or 316 grades. 201 is a high manganese and low nickel stainless steel with low nickel content and poor corrosion resistance. It is widely used in various tabletops, countertops, kitchenware, outdoor decoration engineering, urban decoration industry and low-grade household products. It is also used in medical instruments and automotive parts that require flexibility while maintaining strength under pressure.
Product Parameters
Minimum Order Quantity: | 1 tons |
Packaging Details: | water proof paper is inner packing, galvanized steel or coated steel sheet is outer packing , side guard plate , then wrapped by seven steel belt. |
Delivery Time: | 15-20 days or subject to the clients' requirement and quantity |
Payment Terms: | 30%TT for deposit, 70% balance before shipment or LC at sight |
Supply Ability: | 20000 tons per month |
Chemical Composition
C | Si | Mn | Cr | Ni | S | P |
≤ 0.15 | ≤ 0.75 | 5.50~7.50 | 16.00~18.00 | 3.50~5.50 | ≤ 0.03 | ≤ 0.06 |
Mechanical Properties
Tensile Strength Kb (MPa) | Yield Strength σ0.2 (MPa) | Elongation D5 (%) | Hardness |
≥ 520 | ≥ 275 | ≥55-60 | ≤183HB;≤ 100 HRB |
Physical Performance
Density(g/cm³) | Modulus of Elasticity(Gpa) | Coefficient of Thermal Expansion(10-6/°C) | Coefficient of Thermal Conductivity(W/m*K) | Resistivity(μohm.in) |